This was ready to be shipped when I dropped it while taking a picture for the buyer to decide between this one and another. I do not want to toss this one, way too much labor invested at this point.
The finish is shellac and Johnson's Paste Wax. I can refinish the damaged face if I have to. But I do not think I can sand away the dents and maintain the proper look of the lock, unless I sand the entire lock.
Folks report having raised dents with steam - a steam iron carefully applied over a handkerchief or the like. Never tried it myself, but perhaps someone who has can chime in with details.
but you will need to get the steam to the bare-wood. Will need to remove the shellac in the area of the dents. Sand & reapply the shellac and call it done.
Strip the finish, wet the area for a bit and hold a steam iron on the cotton setting on it. Let it dry, sand and refinish. Due to circumstances supposedly beyond my control, I've used this method quite a bit. I've even done it through an oil finish.
I prefer a soldering iron that I reshaped the tip by hammering flat and then shpaed it to a point with a file. it is smaller than a clothes iron and easier to get the heat where you need it. I have used both cotton rags and paper towels and they both work just fine. It is easier then you might think and very effective as long as the fibers have not been severed.
When hammering the tip on a soldering iron you shoud remove it from the iron first, DAMHIKT.
Before I steam or heat, I usually take a strip of damp paper towel and lay it over the dent. If an application or two doesn't raise the dent, I go for steam.
I often use an old iron I purchased at an auction. I would remove the shellac in the area, apply a few drops of water in the depressed area only. That may swell the area enough that you don't even need to use the steam. If it doesn't add a few more drops and cover with a slightly dampened cloth and apply heat when it steams the dent will usually disappear, if not repeat the treatment. Should not be any problem to then lightly sand the area and retouch with shellac.
very diminishing returns. Once the fibers are swollen they will not respond further. A second application may add a tiny bit of correction but nothing like the first shot. Prepare the area and do it all at once. If you have a test piece try it for heat and time, then go after it. I've had deeper dents pop to normal.
I have hard water - with a small amount of Iron. When I use the steam method I always use distilled water - the iron will react with some woods and cause bad staining. I always keep a few of the Wallmart distilled water jugs in the shop - good for mixing dye and steaming etc.
The long one will easily steam out. A soldering iron and a soggy rag twisted into a tight coil will work. Use plenty of water; the rag needs to be soggy so that lots of steam is made.
The short on looks like the grain is broken. It will partially steam out and you will have to sculpt the remainder to be rid of the broken grain.
Since you'll have to do the finish over anyway, here's a YouTube video by my friend, Charles Neil, that will work too. Have a look to see if this is an option for your situation.
Thanks everyone for the help. I almost cried myself to sleep the evening I damaged this lock. A whole bunch of TLC goes into making one of these. I will not get a chance to try a fix until this weekend at the earliest.
This is a completely wood functioning lock. Even the internal spring is wood. Attached is a picture of the entire setup. The hasp also functions. The curly cherry plaque on the right in the picture is where the damaged lock was supposed to go.
that may be the neatest woodworking I have seen on WC. It deserves to be posted as a separate post for all to admire. These neat locks may be missed by some buried in the repair discussion.
You may need to remove finish to get the steam into the wood. I have never tried steaming something that was finished. There is no doubt that the long scratch will quickly steam out. I suspect the smaller dent may not be completely removed. I would fill what is left with a dark shellac stick filler and make it look like some dark colored spot that might be naturally occurring in the wood.
I hit the piece with a air drier after steaming to dry out the steamed place. If you sand it too quick before the wood dries you will be left with a hollow spot.
You may wonder how it is that I have so much experience fixing screw ups. I'm not telling........
before this but since they didn't I will. Where do you sell these? Is there a photo shot of the inner workings? I'm assuming that the spring is a lever style spring. Nice work and I for one would like to see more. By the way how do I reach you? You can email me if you like through this site. The injured one interests me.